    Does anyone know what mixing ratios are used with the PPG DP epoxy primers? Do these use a hardener or is everything included in the reducer/catalyst?

    Thanks,

    Flattop
     
  2. SpeedRacer2002
    Joined: Jan 11, 2002
    Posts: 777

    SpeedRacer2002
    Member

    been a while but 4:1 seems right and your catalyst is your hardner
     
  3. jusjunk
    Joined: Dec 3, 2004
    Posts: 3,138

    jusjunk
    BANNED
    from Michigan

    Ever try google? all the info is online. I just dont have the link handy here at work..
    Dave
     
  4. CMenard
    Joined: Nov 18, 2006
    Posts: 36

    CMenard
    Member

    4:1 with the catalyst. I spray it 4:1:1/2 part DT reducer.
     

  5. Flattop
    Joined: Mar 13, 2005
    Posts: 153

    Flattop
    Member

    Many thanks!

    Flattop
     
  6. LUCIFR
    Joined: Mar 8, 2006
    Posts: 634

    LUCIFR
    Member
    from Seattle

  7. SlowandLow63
    Joined: Sep 18, 2004
    Posts: 5,953

    SlowandLow63
    Member
    from Central NJ

    Ditto ^^^ You can always check PPG's tech sheets at PPG.com They'll give you mixing ratios, proper substrates, flash times, etc. Basically whatever you need. I printed out the ones I use the most and keep them in a binder with the rest of mine.
     
  8. I hope you didn't shoot your car yet. The mix is 2 to 1 not 4 to one. 2:1:1/2 if you want to use it as a sealer. It needs a 30 min dwell time if you use the 401 catalyst. If you don't have a P sheet, you might want to look at the side of the can.
     
  9. Sam F.
    Joined: Mar 28, 2002
    Posts: 4,225

    Sam F.
    BANNED


    yes!

    http://www.ppg.com/cr-refinish/phase1/frmProductInfo.asp

    type what ever product you are using in the box to the left,,,all your online P sheets ,,print hem out,,share with a friend :D
     
  10. Flattop
    Joined: Mar 13, 2005
    Posts: 153

    Flattop
    Member

    I was able to get in touch with a PPG distributor who told me to go with the 2:1 ratio. I have had this stuff for about 4 years now and had long ago lost the tech sheet. I appreciate everyones' responding.

    Thanks,
    Flattop
     
  11. Sam F.
    Joined: Mar 28, 2002
    Posts: 4,225

    Sam F.
    BANNED

    well,,,i hope your cataliyst has never been opened,,,,because if it has then its gone bad,,,,
     
  12. LUCIFR
    Joined: Mar 8, 2006
    Posts: 634

    LUCIFR
    Member
    from Seattle

    I beleive the 2:1 ratio is for a real fast flash off?? if thats what you are looking for??
     
  13. Sam F.
    Joined: Mar 28, 2002
    Posts: 4,225

    Sam F.
    BANNED


    dude.the ratio is 2:1....thats what it is...
     
  14. prl98
    Joined: Apr 16, 2007
    Posts: 103

    prl98
    Member

    is dp or dplf? the mix ratio is different. dplf is 2:1. the old dp is 1:1. If you want to use as asealer then you would mix dplf at 2:1:1, and dp at 1:1:1/2
     
  15. Sam F.
    Joined: Mar 28, 2002
    Posts: 4,225

    Sam F.
    BANNED

    you can still get DP in california???

    thats wild,,,cant even get it here in kentucky and cali's regulations are the reason for dpLF (lead free)....
     

Share This Page

Register now to get rid of these ads!

Archive

Copyright © 1995-2021 The Jalopy Journal: Steal our stuff, we'll kick your teeth in. Terms of Service. Privacy Policy.

Atomic Industry
Forum software by XenForo™ ©2010-2014 XenForo Ltd.