    I found several quarts of DP40lf primer that I'd like to use. What activator do I need?
     
  2. FunnyCar65
    Joined: Mar 11, 2007
    Posts: 2,092

    FunnyCar65
    Member
    from Colorado

    DP401LF or DP402LF
     
  3. 400 4spd.
    Joined: Jan 23, 2011
    Posts: 49

    400 4spd.
    Member

    Note that the 401 hardener has to be added at least 1/2 hour before it can be sprayed. The 402 does not have an induction time required and can be sprayed right away. Pot life is also longer with 401.
     

  4. 40fordtudor
    Joined: Jan 3, 2010
    Posts: 2,503

    40fordtudor
    Member

    that's good to know---thanks.
     
  5. towithome
    Joined: Oct 22, 2012
    Posts: 42

    towithome
    Member
    from oregun

    Use the 401, it makes dplf a decent epoxy. Avoid the 402.
     

Share This Page

Register now to get rid of these ads!

Archive

Copyright © 1995-2021 The Jalopy Journal: Steal our stuff, we'll kick your teeth in. Terms of Service. Privacy Policy.

Atomic Industry
Forum software by XenForo™ ©2010-2014 XenForo Ltd.