The Jalopy Journal
U would have to clear it and then San and apply candy, wouldn't flake it, it will kill the effect.
looks good. nice flow.. nice use of blues.
theres no urethane sealer that goes directly over bare metal.. pre treatment such as a etch primer or epoxy is needed... is it catalyzed...
are u balling that much u would use a brand new spray gun that just barely came out for just flake? a 1.3 will have a tough time spraying a...
give me a run down of your steps.. from primer up. base, midcoat with flake or 2k clear with flake.. regular clear. flash time.. gun used info...
the main reason is the cost and skill to pull it off.. the ones who cant afford it say how gawdy it is and how much they love there rustoleum...
x2 and pearl is an effect.. sometimes u need a pearl basecoat 2 stage.. or sometimes u need a tristage pearl with a certain groundcoat.. or...
wear gloves and a spray suit.
Never mix pearl in a topcoat clear.. It's a pain in the ass.. No dry spraying from 2feet away unless u want ur paint job to delam.... Mix pearl...
crushed glass is ice pearl.. u can find it from hok.. its finely ground glass.. comes in white, blue, red, purple and maybe one other color.. not...
good job mitch! u just left out the part from clear to stripe.. the all important one.. LOL
cool board.
no pics of vandemon doing the layout? what it take him like 3-4 hours both sides? p.s. i know im quoting a 3 year old post
the way i do flames or any graphic is.. first start off with a non catalyzed base. i usually hok, sem, or other bases sometimes. shoot base, shoot...